Swen,
The best known supplier for DBC would have to be Curamik, there
main office is in Germany, and offer a range of DBC products (Tel
+49-96 45-92 22 0 for nearest office ) Within the UK I have also had
subs from both Advanced Inetreconnection Technologies (AIT) and IXYS
(the die supplier) but dont have contacts for either, sorry.
One thing I will say is that I have had problems with AlN DBC
cracking through the ceramic during thermal testing, Alumina also
does this, but the AlN fails far earlier.
Good luck
Roger
______________________________ Reply Separator _________________________________
Subject: [TN] Alumina & AlN DBC substrates needed!
Author: [log in to unmask]@INTERNET at #EMAIL
Date: 11/09/98 12:39
Message authorized by:
: [log in to unmask]@INTERNET at #EMAIL
Dear all,
We're going to purchase some Alumina DBC substrates as well as some AlN
DBC substrates for our project. Does someone have some information about
this? The dimension of these substrates is 2"x 2" x 0.025", both sides
coated with ~10 mil copper, Alumina and AlN dielectric layer is around
20 mil. Thanks for your attention.
wen
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text
in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for
additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700
ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|