I have two suggestions. One has already been suggested and that is to keep
the coated cards away from elevated temperatures as long as possible. The
second suggestion is to thin the conformal coat which allows the entrapped
air to escape easier. Jon
----------
From: Lum Wee Mei [SMTP:[log in to unmask]]
Sent: Monday, August 31, 1998 9:27 PM
To: [log in to unmask]
Subject: [TN] Bubbles from conformally coated board
The test engineer came back to us to complain that bubbles are found
along the edge of the power modules after going through the
temperature
cycling tests. This problems are found on both coated boards. The
power
modules are mounted completely flushed onto the board and subject to
conformal coating using the diping method. The coated board undergo
QC
to ensure all components are completely coated, inlcuding the edges
around the modules.
What could be the problem?
################################################################
TechNet E-Mail Forum provided as a free service by IPC using
LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|