read all the mail in regards to thiss topic - everything sounds fine n dandy -
but everything mentioned will not give a constant striiping speed - or if the
speed is constant - it cannot be - let's say - at a speed in proportion to the
etcher n tin stripper - and how long wud it last. just spent over 18 months
working on whole process tie in - controls and effects. the actual kind of dry
film has an effect on it also. this industry has failed in the last few years
to actually understand the complexity of it all - lot more to it than having
proper control or straight chemistry itself
Rick Fudalewski
Atotech Canada
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################