Hi and thanks for reading this message.
Has anyone experienced solder "webbing" or "sticking" to the permanent solder
mask on boards after wavesolder? I'm seeing it on some products but not on
others. I suspect that it is uncured solder mask but wanted to get some other
opinions.
Thanks in advance,
Mike
################################################################