Are these "dimpled" BGAs? Are the component pads recessed below the bottom
surface? If so, perhaps you might try screening the flux instead of
dispensing. This might give you a better flux deposit without voids.
Jim Marsico
AIL Systems Inc.
(516) 595-5879
[log in to unmask]
Fumiaki Shigeoka wrote:
My problem is dropping solder ball from BGA devices after ball attachment
process.
First, I suspected the temperature of reflow oven, but that was sufficient to
melt
solder ball. After reflow, some balls(5-10% of strip) are missing, and empty
pads
are not wetting or partially wetting.
I found voids in flux on pad before placing ball, so I guess the void will
expand
in reflow furnace, and ball doesn't touch to pad. I use dispensing system to
provide
flux, which sometimes contaminates air void to flux on pad.
Does anyone have any experiences and suggestions to solve this problem ?
Thanks in advance.
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|