Dear Technetters,
Recently, we faced a solderability problem on our fab. I have the following
questions for assembly houses.
(1) How many assembly houses perform solderability test using solder-sample
fab?
(2) Is there any information as how effective this test is? I mean any lot
went bad still after doing solderability test (at assembly house).
My management wants to know the overall industry trend and effectiveness of
the test to make decision.
re,
Ken Patel
______________________________________________________
Ken Patel Phone: (408) 490-6804
1708 McCarthy Blvd. Fax: (408) 490-6859
Milpitas, CA 95035 Beeper: (888) 769-1808
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|