Hi Earl,
The best way I've found to transfer solder is using those large egg cartons
that McDonalds et al get their eggs supplied in. The solder doesn't burn
the material (surprisingly) and when cooled the solder 'eggs' just drop
right out in a good size for your new pot - a good size for melting from
cold that is......
Best Regards
Justin Braime
Production Engineering
Alpine Electronics of New Zealand Ltd
------------------------------------------------------------
15a Vestey Drive, Mt Wellington,
Private Bag 14921, Panmure,
Auckland, New Zealand.
Phone: +64-9-573 7100
Fax: +64-9-572 7101
-------------------------------------------------------------
----------
> From: Earl Moon <[log in to unmask]>
> To: [log in to unmask]
> Subject: [TN] Seho Wave Soldering Process Procedures
> Date: Saturday, 19 September 1998 04:05
>
> We have our Seho 2135F almost ready to run. Have a few questions
> concerning operating tips, startup procedures, do's and dont's, safety,
> etc.
>
> Also would like to know, as our solder pots were damaged during shipping
> (750 and 950 kg - wonder why the damage), what the best way to get the
> old solder out of the damaged pots and into the new ones.
>
> Any information greatfully received,
>
> Earl Moon
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
> ################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|