Mike Manwell <[log in to unmask]>
Date:
Wed, 16 Sep 1998 07:48:12 -0700
Content-Type:
TEXT/PLAIN; CHARSET=US-ASCII
MIME-Version:
1.0
Reply-To:
Parts/Attachments:
TEXT/PLAIN (57 lines)
This is very helpful, I appreciate your response as well as everyone else who
has responded.
Thanks again,
Mike


On Wed, 16 Sep 1998 04:34:08 -0700 Hoppa, Floyd wrote:

> From: Hoppa, Floyd <[log in to unmask]>
> Date: Wed, 16 Sep 1998 04:34:08 -0700
> Subject: [TN] Flux Measuring Techniques
> To: [log in to unmask]
>
> One method we use for this measurement is a specially designed carrier
> with (4) glass plates in slots held down by spring clamps.  These plate
> glass pieces are removable.  The following steps are then taken:
>         1) We will wash the plate glasses and pallet.
>         2) Weigh the (4) glass plates separately and record the weight.
>         3) Assemble the glass plates into the pallet.
>         4) Run the pallet down the wave solder machine (chip wave and
> wave bath are off)
>         5) Remove the glass plates and weigh in the scale.  Record the
> data.
>
> The scale is measuring (or attempting to measure) micrograms.  We use a
> Ainsworth 1000 scale (which run approximately ($70,000).  We will run
> several tests to see if it is repeatable and consistent.
>
> Hope this helps.
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
> To subscribe:   SUBSCRIBE TechNet <your full name>
> To unsubscribe:   SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
> ################################################################
>

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2