I would look into a glass plate. I use it as a part of my process control. You
can either use it or look into putting a piece of thermal paper on the topside
of a bare panel and run it through. You should then see the paper wetting, and
you know you have good fluxing to the topside. When you use the glass plate you
want to watch for three things.
1. After fluxing, make sure you have an even thin coverage with no stips or
overlaps.
2. After preheats, you want to make sure that your solvent did "just"
evaporate.
3. You want to watch it as it goes over the wave to assure the flux is doing
it's job. Not too much nor not enough. If you hear alot of crackling as it
goes over the wave, you know you've applied too much, because it didn't
thoroughly evaporate all the solvent. I hope this helps a little.
Mike Manwell <[log in to unmask]> on 09/15/98 07:04:25
PM
Please respond to [log in to unmask]
To: [log in to unmask]
cc: (bcc: Jason Smith/Lex/Lexmark)
bcc: Jason Smith/Lex/Lexmark
Subject: [TN] Flux Measuring Techniques??
We are using a sprayfluxer in our wavesolder operation and Im wondering if
anyone has a good method of "measuring" the amount of flux to ensure
consistency. Any help would be appriciated.
Thanks in advance,
Mike Manwell
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text
in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for
additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700
ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|