I would have to say you are correct, the testing for opens on
BGAs is difficult, even with the HP 5DX machine we have here. I can't
recall having seen a single open joint on a properly reflowed
collapsible BGA, but we have seen them on non-collapsible.
How would you attempt to verify that the package is parallel to
the board surface? I know some of the OMPAC plastic packages that we
use will occasionally be lower in the center than the edges, although
not by very much.
I look forward to other comments from Xray users about this
subject.
Paul Quintin
Data General
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|