Hello all,
Mary. We wave solder a lot of 1206's. Our standard pad config is 2/3 the
width of the part and has been for about 15 years. Every year or so,
someone comes along and says we should change our pads to 'IPC Standards'.
Where is it documented that the footprint should be 2/3 of the width of the
part? It would be nice to have a better response than "trust me, this is
what you want".
Thanks,
Chris Ball
ITT Automotive (formerly Delco Chassis/ soon to be Valeo)
.................
A different footprint is required for wave soldering than is for
reflow soldering. The wave solder footprint must be narrower to
minimize the amount of solder that is retained. For wave soldering,
the width of the footprint should only be 2/3 of the width of the
part. During wavesoldering, the solder should form a nice concave
and feathered joint at each end of the component. The solder joint
should not be bulged nor should it build up over the top of the
termination.
..................
################################################################
DesignerCouncil E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE DesignerCouncil <your full name>
To unsubscribe: SIGNOFF DesignerCouncil
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|