Hi Jim,
I'm no BGA expert, but I would think you would tend to experience dendrite
growth on anything that doesn't get cleaned properly. Some people may have
equated this to BGA's since it may be harder to clean thoroughly under some
of them. I would thank that if you get the cleaning down pat, the dendrite
thing would go away.
Good luck in your new role. ; > )
Charlie B.
[log in to unmask]
Jim Marsico 516-595-5879 <[log in to unmask]> on 08/20/98 03:07:00 PM
Please respond to "TechNet E-Mail Forum." <[log in to unmask]>; Please respond
to Jim Marsico 516-595-5879 <[log in to unmask]>
To: [log in to unmask]
cc: (bcc: Charles Barker/US/I-O INC)
Subject: [TN] BGA'S IN SPACE
Dear Experts:
I've been asked to investigate this concern, so here goes:
When someone in my company mentioning using BGAs for a space application,
one
of our customers raised a concern about dendrite growth. Unfortunately,
this
is the only information I have. I don't know any specifics regarding the
assembly or the application (or the customer, for that matter) or where or
what
kind of dendrites. All I know is that I'm now deemed the "company expert"
on
BGAs, so I got the task.
Has anyone heard of a dendrite growth problem associated with BGAs?
Thanks for your help.
Jim Marsico
AIL Systems Inc.
(516) 595-5879
[log in to unmask]
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|