High Phosphorous Nickle platings are difficult to impossible to solder to
without the use of acid fluxes. my recollection is that the low phospher
plating bath should be < 3-4% Phospher for successfull soldering ability.
Further given a low Phospher formulation Nickle oxides readily and again
will not be readily solderable with Organic acid fluxes. To prevent
re-oxidation of the Nickle the plater should thoroughly clean following
the Nickle bath and then immedialty overplate with 50-100 micro inches of
soft Gold I.e no brightners, hardners etc. The alternative is to hot
solder dip the Nickle to prevent re-oxidation of the lead.
since you are already having trouble intermittently sometime being able
to use a Rosin flux and sometime requiring a OA flux I assume the leads
already have a Gold finish as is the customary practice. solderability
problems are common with Gold finishes if not properly performed ,
causing the Gold to be porous and thus allowing the Nickle beneath it to
re-oxidize. The presence of organics due to poor cleaning will usually
evidence itself by forming pin-holes when soldered.
good luck
Jess
_____________________________________________________________________
You don't need to buy Internet access to use free Internet e-mail.
Get completely free e-mail from Juno at http://www.juno.com
Or call Juno at (800) 654-JUNO [654-5866]
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|