Jim, I've seen the same "anamoly" in multilayer boards. The areas in question were the same on every board, but did not seen to spread or propagate during our (limited) temp cycling. We felt it was delamination due to thermal stress from a particularly hot component (PTH installation) adjacent to a large buried ground plane. However, neither our cross-sections or those of our board supplier showed any evidence of actual delamination or disbond in the cross-sections, ie no areas of separation. The cross sections did (in our opinion) have some areas which appeared to be resin starved, but we couldn't reject them on that. The boards did not fail during our testing but we were still concerned about long time reliability. We ended up scrapping the boards and remaking them in a higher Tg laminate. The "anamoly" went away ...
Sheila @ Tracor AES
----------
From: PELCHAT_JM[SMTP:[log in to unmask]]
Sent: Friday, August 14, 1998 9:15 AM
To: [log in to unmask]
Subject: [TN] Wavy board surface - NOT delamination?
We have a 12 layer board with a heavy ground layer that had
three edge BNC type connectors installed using a mini wave.
The circuitry tracing away from the connectors is surrounded by
vias. There is a distinct lightening of the board material I
have typically associated with measling. This lightening
however, doesn't have any fiber crosshatching I am used to
seeing with measling, not does it look like classic
delamination. I have documented the event as delamination for
lack of a better description.
The opposing consensus is that it is "merely" soldermask
discoloration. Without classic delamination or measling
features, I don't feel I have a leg to stand on to call it
anything other than that. (Don't worry though - both sides feel
the Customer needs to review the board no matter WHAT the defect
is).
Does anyone have any opinions?
Jan Pelchat
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|