Mime-Version: |
1.0 |
Sender: |
|
Subject: |
|
From: |
|
Date: |
Tue, 25 Aug 1998 22:47:48 EDT |
Content-Transfer-Encoding: |
7bit |
Content-Type: |
text/plain; charset=US-ASCII |
Reply-To: |
|
Parts/Attachments: |
|
|
Hi Howard,
It depends what it is you want to be doing. MIL-STD-202F thermal cycling was
fine for hybrid assemblies or bare PCBs, but a disaster for SM assemblies,
because it was outside the temperature ranges for near linear temperature-
dependent property changes. For SM assemblies look at IPC-SM-785.
Werner Engelmaier
Engelmaier Associates, L.C.
Electronic Packaging, Interconnection and Reliability Consulting
7 Jasmine Run
Ormond Beach, FL 32174 USA
Phone: 904-437-8747, Fax: 904-437-8737
E-mail: [log in to unmask]
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|