In a message dated 08/24/98 7:16:37 PM Pacific Daylight Time, [log in to unmask]
writes:
> Will there be any problem if my board surface finish is OSP and has a
> press-fit connector?
>
> Re,
> Ken Patel
Hi Ken!
None that I'm aware of...but I guess it really depends where your board is
going to be living the rest of it's life...I suppose there isn't really any
more of a risk for problems than there is with a plated barrel. Although it IS
pretty important that your finished holes are a good fit with the press fit
pins, cause you don't have that "fudge factor" of the plating anymore.
At a past employer, we built quite a few different assemblies for a major
networking company here (hint: they're by great america), that used quite a
few high density right angle press-fits because these boards plugged into
backplanes. After a faux pax or two,...or three,...okay then, four...we got
pretty good at it...(learning curve...you know how it is). One thing
important, a good stable fixture, as well as a precisely drilled support plate
accurately supporting the laminate close to the barrels will keep them from
getting pushed out of the board. I don't know how you're doing this, manually
with an arbor press, or with some sort of automated press, we just used a
manual arbor press. Interestingly enough, we found out that we had less barrel
damage when we had our ladies doing it rather than the guys...more delicate
touch I suppose?
-Steve Gregory-
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|