My book only goes to 70/30 (tin/lead). need help. Our part supplier is using
90/10 rather then 63/37. The higher tin causes more oxides creating some
cold solder joints. Supplier has brass base followed by copper flask and
90/10 tin/lead. What is the liquidus temperature of tin/lead of 90/10 and
has anyone had the experience. Also the feet to this part are very small and
close to the pad. Hard to inspect. We had the supplier go to 63/37 and had
very little problem. Supplier wants to go back to 90/10. whats the
concensus?
################################################################