We ran a trial batch of boards using this finish instead of our standard
Au/Ni finish employed for mixed and SMT PCBs. Omikron finish would have
been around 8% cheaper from our supplier had we swapped over.
Results were very good through both SMT and wave solder process, however
some solderability problems with subsequent hand soldering operations
(we require a few select-on-test resistors to be fitted to each board.)
Also minor disadvantage that the inspection benefit from colour contrast
between pasted land and unpasted land of Au/Ni finish is lost. Better
than HASL for SMT assembly though.
Nigel Burtt
Production Engineering Manager
D - European HQ
Email: [log in to unmask]
Tel: 01793 842132
Fax: 01793 842101
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|