William -
I recently had the opportunity to test the KIC SlimKIC II and Autopredict
software for a client of mine. Having done reflow profiling for the last
century or so I was skeptical of the "autopredict" function. This was
compounded by having played with other attempts at profile prediction in the
past. Suffice it to say I was very pleased with the KIC autopredict software.
I threw some easy and some complex assemblies at it (in terms of overall mass
and surface geometry compexity) and it did a very good job. I strongly
recommend that you try it out on your own PCB applications. I think you will
be pleased with the performance.
Phil Zarrow
ITM, Inc.
Durham, NH
www.itm-smt.com
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|