Try Morton 5050 from Dynachem
Lourdes
>>> Zecal Engineering <[log in to unmask]> 08/19 10:52 AM >>>
We have trouble with dry film lifting during heavy dep gold plating. LPI works, but is difficult to strip. Any suggestions?
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################