Because of a vendor mis-hap we recieved pcbs with palladium and not
tin plating. We use a 2% silver solder so it is a good match. We are
concerned with any long term effects i.e. corrosion.
Can some of you please respond with your experience
with palladium and pcbs. Don Fumia "
---------------------------------------------------------------------------
------------------------------------------------------------------
Hi,
We have made some preliminary trials with Palladium Process called "
electroless palladium "
by Atotech, with formic acid as the reducing agent.
I suppose there is also a process called " immersion palladium ".
Personally I think it gets too
thin and it is preferrably used as a activator in Ni/Au- processes, for
example.
Well, in our case it worked fine, we are pleased with solderability. We
have not made environmental tests
& other tests so far, personally I think that corrosion is not a problem,
because palladium is the most
noble metal and hence it is almost impossible to get it corrode.
The real problem of palladiumin our case is availibility/price fluctuation
in Europe.
Brs, Johannes
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|