Dennis,
Commercial forming gas is typically 5% hydrogen. It's used to
prevent/reduce light oxidation, but I never found it to be very
effective because of the inevitable mixing during the purge cycle. If I
remember right the explosive mixture limit is 8% hydrogen. There's also
an upper limit that I forget the value of where you're safe again, and
that's where hydrogen furnaces operate.
We used to crack ammonia to create a "pure" hydrogen atmosphere in the
hot zone for making hermetic glass seals. The conveyor portals were
blanketed with nitrogen. We had a few interruptions in the nitrogen that
automatically cut off the hydrogen, but you still get quite a boom out
of the residuals.
Andy Magee
Flex Guru
[log in to unmask]
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|