The reduction mixture recommended is upto 5% hydrogen and beyond that
safety is of concern.
We never used beyond 5% hydrogen and thus made no special safety
arrengements except standard gas handling requirements, explosion proof
cylinder chamber, fire extinguisher nearby.
ashok
> ----------
> From: [log in to unmask][SMTP:[log in to unmask]]
> Sent: August 17, 1998 1:39 PM
> To: [log in to unmask]
> Subject: [TN] Hydrogen/Nitrogen saftey issues
>
> From: Dennis J Fall@TFT on 08/17/98 01:39 PM
>
>
> To: [log in to unmask]
> cc:
> Subject: Hydrogen/Nitrogen saftey issues
>
> I am looking for some information regarding the safety of reflow ovens
> using a 15% Hydrogen 85% Nitrogen atmosphere. If anyone has had
> experience
> using this concentration or something close to it, please let me know.
> Maybe we can discuss any safety issues that may pertain to the
> process.
>
> Thank You,
>
> Dennis Fall P: 507-625-8445 x17
>
> Process Engineer F: 507-625-3523
>
> Thin Film Technology Corporation mailto:[log in to unmask]
>
> 1980 Commerce Drive http://www.thin-film.com
>
> North Mankato, MN 56003-1702
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
> 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
> section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or
> 847-509-9700 ext.312
> ################################################################
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|