Mark: The maximum service temperature for unfilled optically clear epoxy is
about 180 C. It "may" survive short exposures in the reflow oven of the 250 C
range without yellowing or breaking down but you're pushing it. You may want to
consider a clear silicone system which has better high temperature resistance.
As far as moisture absorption most high temp unfilled epoxies should be less
than 0.5% B.W. Is this good enough to meet your requirement?
The issue of air bubbles is up to you to control. This will probably require a
vacuum de-airing step of the material prior to encapsulation and possibly
another one after, prior to cure.
Contact: Grace Speciality Polymers; Atlanta GA. 404-696-4565
MasterBond Inc. Hackensack N.J. 201-343-8983
TRA-CON Inc. Medford MA. 617-381-5550
Regards
Michael Barmuta
Staff Engineer
Fluke Corp.
Everett Wa.
425-356-6076
On Tue, 11 Aug 1998 13:20:04 -0700 Mark [log in to unmask] wrote:
> From: Mark [log in to unmask]> Date: Tue, 11 Aug 1998 13:20:04 -0700
> Subject: [TN] Optically transparent epoxy
> To: [log in to unmask]
>
> Technetters,
>
> I am looking for an optically transparent epoxies for use as a potting
> compound that can withstand IR reflow. This epoxy must be very stable and not
> absorb moisture. Also air bubble must be kept to a minimum. Recommendation
> on manufacturers, suppliers, or specific products would be much appreciated.
> Also any information on reliability of these products would be also help.
>
> Thanks for your help,
>
> J. Mark Elliott
> Maxtek Components Corp.
> 503.627.3641
> [log in to unmask]
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
> ################################################################
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|