There exists a phosphorous problem. Beyond that, it is inadvisable to
solder to any nickel surface - that is: No solder termination area
should be bare nickel. It should be coated or plated over with a metal,
or other surface finish, not allowing its normally very rapid oxidation.
More often now, people are talking about the deleterious affects
phosphorous, and some other components in the electroless coating
process, have on solderability, solder joint acceptance, and long term
reliability. There have been many discussions on this forum and in
others as the SMTNet.
Under electroless gold, phosphorous goes to the solder termination area
surface and forms intermetallics in amounts causing the problems
mentioned. This is according to some SMD suppliers and others
investigating this phenomonon.
Earl Moon
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|