Hi Matt
The prepreg can be kitted and QC inspected, or even weighed, before it gets
into the layup room. rather than letting the layup people pull it themselves
from a stack.
And the final boards can be 100% thickness measured after lamination so that
you don't see the ones that are too thin.
################################################################