Yes, MIL-STD-202F is good testing condition for bare PCB. But I look
up IPC-TM-650 to find thermal cycling condition. It is as same as MIL's
but qualification criteria is different. Which should I follow? Do you
think it is possibleto satisfy the requirement of FR-4 thermal shock
according to IPC-TM-650 if I use air to air chamber?
Howard Lin
Maxedge RD Center
> -----Original Message-----
> From: Werner Engelmaier [SMTP:[log in to unmask]]
> Sent: Wednesday, August 26, 1998 10:48 AM
> To: [log in to unmask]
> Subject: Re: [TN] Thermal Cycling
>
> Hi Howard,
> It depends what it is you want to be doing. MIL-STD-202F thermal
> cycling was
> fine for hybrid assemblies or bare PCBs, but a disaster for SM
> assemblies,
> because it was outside the temperature ranges for near linear
> temperature-
> dependent property changes. For SM assemblies look at IPC-SM-785.
>
> Werner Engelmaier
> Engelmaier Associates, L.C.
> Electronic Packaging, Interconnection and Reliability Consulting
> 7 Jasmine Run
> Ormond Beach, FL 32174 USA
> Phone: 904-437-8747, Fax: 904-437-8737
> E-mail: [log in to unmask]
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
> 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
> section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or
> 847-509-9700 ext.312
> ################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|