Try ANSI/J-STD-001B, Page 17, paragraph 9.2.5.1, second sentence. "Single
sided boards (unsupported holes) shall meet conditions C & E of Table 9-1.
Table 9-1 requires 75% land\pad coverage and 270 degrees of lead wetting (330
on class 3).
Steve Mikell
SCI Systems
>Can somebody enlighten me which IPC standard tells the acceptance criteria
>of solder joints in a thru hole assembly of single-sided PCB (no PTH).
>
>Thanks!
>K.K. Chin
>Artesyn Technologies
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|