Could you share test data regarding solderability on each
condition with me. From our beaker test Omikron White Tin
showed better result than Dexter's. And what about cost
factor ? As far as I know, if HASL has 1X, 0.6 X for OSP,
1.4 X for Tin and 4.0 X for Immersion Gold.
There is a tendency towarding Immersion Gold, but in the
standpoint of PCB shop too much burden because most
our customer want us kept same price as HASL's. In that
case we have to loose our profit at least $1.0/board ( $
10/ sq. meter).So White Tin seems to me very attractive.
I
J.H.Lee
R & D Director
Daeduck ELectronics Co
[log in to unmask]
fax: + 82-345-81-8246
tel : + 82-345-81-8191
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|