Folks,
We are converting an assembly from HASL to gold that has large
quantities of 20mil devices. With HASL boards, we used a rule of thumb
of 2mil off of aperture width on these parts, 1mil on each side. Based
on the lack of pre-existing solder, should we go 1:1 on the gold board
stencil apertures? One of our engineers is recommending this, but I am
concerned about the possibility of bridging on 14mil wide pads. Our
stencils are 6mil laser cut/electropolish. Any insights would be
appreciated....
Mike McMonagle
PCA Process Engineering Supervisor
K*Tec Electronics
1111 Gillingham Lane
Sugar Land, TX 77478
(281) 243-5639 Phone
(281) 243-5539 Fax
[log in to unmask]
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|