David D Hillman <[log in to unmask]>
Date:
Thu, 20 Aug 1998 06:47:20 -0500
Content-Type:
text/plain; charset=us-ascii
Reply-To:
"\"TechNet E-Mail Forum.\" <[log in to unmask]>, David D Hillman" <[log in to unmask]>
Parts/Attachments:
text/plain (141 lines)
Hi TechNet! Sorry Lenny but the paper you reference doesn't support the
clam that Al wirebond on ImmAu/ENi is acceptable. Table 4 on page 691and
the associated discussion details successful Au wedge bonding on ImmAu/ENi
but not for aluminum. There have been some reports of successful Al
wirebonding on ImmAu/ENi (as soon as I can dig up the reference out of my
files I'll post it on TechNet) but not that specific reference.


Dave Hillman
Rockwell Collins
[log in to unmask]




Lenny Kurup <[log in to unmask]> on 08/11/98 09:20:02 AM

Please respond to "TechNet E-Mail Forum." <[log in to unmask]>; Please respond
      to Lenny Kurup <[log in to unmask]>

To:   [log in to unmask]
cc:
Subject:  Re: [TN] Is Al to Ni wirebonding possible




Hello Rusty,

Consult "Wirebondability and solderability of various metallic finishes for
use in printed circuit assembly."  by Hillman, Bratin and Pavlov; 1996 IPC
Expo, S.J.

Results have shown peel strengths to be way below IPC wirebondability
requirements, for Al wire on elNi/ImAu. Au wire, however, passes the peel
strength requirement.


Regards,

Lenny Kurup
EMX Enterprises Ltd.
Markham, Ontario, Canada
905-475-8000 Ext 240.




On Tue, 11 Aug 1998, Rusty Boyd wrote:

> Hi,
> A certain vendor claims that thermosonic Al to Ni wirebonding is
possible. I am
> looking for references to refute or support this claim. The precise claim
is
> that on a flexible PCB constructed of:
> Kapton:    25 um
> Cu:        7-8 um
> Ni:        1.0 um
> Au:        0.2 um
> that thermosonic wire bonding with Al wire results in a wire bond to the
Ni
> layer. This claim was made after being confronted with the IPC
recommendation
> that at least 1 um of Au is required.
> If anyone could share his/her experience(s) on this subject, or, better
yet,
> point me toward some authoritative reference(s), I would greatly
appreciate it.
> TIA,
> Rusty
>
>
>
>
>
> Rusty Boyd
> OUHEP - http://oua4.nhn.ou.edu/
> [log in to unmask]
> office: (405)325-2890 x36316
> office fax: (405)325-7557
> home ph., fax and data: (405)447-5211
> University of Oklahoma
> Dept. of Physics and Astronomy
> 440 W. Brooks
> Norman, OK 73019
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in the body:
> To subscribe:   SUBSCRIBE TechNet <your full name>
> To unsubscribe:   SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
> ################################################################
>
>

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2