At 14:21 18/08/98 -0400, you wrote:
>To TechNet Forum Members,
> We are a contract manufacturer who assembles boards in a high mix
low to medium volume environment.
>Questions:
>What PWB manufacturing process could be causing this?
>There is no evidence of measling which is usually evident after gross
Z-axis expansion, is there something we can do during the assembly
process to help minimize Z-axis expansion?
> How would you proceed with this situation?
Mark ,
From our own experience , as PCB manufacturer , this is not your foult . The
problem exists allready in the boards .
First of all , locate the open via and perform crossection . It will give
all answers .
There are a lot of reasons for such opens .
The most important point to your consideration : opens in small vias found
after assembly are indicating , that reliability of finish boards is not
good . You might be in situation , that there are a lot of opens in copper
and only solder inside the hole create electrical connection .
Send the boards to inspections .
Good lack
Edward Szpruch
Eltek Ltd - Israel
Tel 972 3 9395050
Fax 972 3 9309581
E-mail : [log in to unmask]
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|