Tom,
We've been using Kleenox for about two years. It works very well for
us. Makes de-drossing the pot a lot easier and reduces the solder
waste. I have not noticed any residues in the pot. We send out for
samples every month and I have a spreadsheet of the samples to track any
spikes or irregularities. Flat as a pancake.
Costwise, it ain't cheep, but it works, and we go through a jar a month.
I buy it by the case of 24.
Make sure your operators wear their respirators when handling the
Kleenox. Also, don't throw the empty jars in the trash. They are
HAZMAT items, (at least in California). We have a Safety-Clean
degreaser and we rinse the jars out and then we junk the jars.
Otherwise they have to go through HAZMAT waste disposal.
Hope this helps,
Jared Lang
> ----------
> From: Moss, Thomas[SMTP:[log in to unmask]]
> Reply To: TechNet E-Mail Forum.;Moss, Thomas
> Sent: Monday, August 03, 1998 1:28 PM
> To: [log in to unmask]
> Subject: [TN] Questions about KLEENOX "P"
>
> Hello all,
> I've been lurking on the list for awhile, but I thought I'd
> come
> out of hiding to ask some questions.
> I want to try some Kleenox "P" to reduce the amount of dross
> from our Wave Solder pot. Does anyone out there have any good or bad
> experiences with its use? Will its repeated use leave a residue or
> contamination in the solder? Are there any downsides that I'm not
> thinking of? Lastly, was it cost-effective for you to use?
>
> Thanks in Advance,
> Tom Moss
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
> 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
> section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or
> 847-509-9700 ext.312
> ################################################################
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|