Paul, conductive compounds ("ink") suppliers also include Dupont,
Methode/Chicago, Ormet Corp./
Carlsbad, Calif. (a 706 A/C, no. of San Diego), etc. I have a more
complete list at another location, fax me (619-549-4292) if you'd
like it.
George Gregoire, Pres., Dimensional Circuits Corp.
(DCC is the inventor of IMPRINT Patterning, an advantageous &
emerging method of patterning high density PWBs with microvias & fine
lines. We are also interested in conductives, as Imprinted circuits
can have their vias made conductive at the same time x-y traces are
being made conductive, simply by squeeging in the conductive, which
fills both areas at the same time.) GG
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|