There are two basic methods that fluxes use to eliminate oxidation, they
either dissolve it into "solution", or they reduce it back to the metal.
If it is reduced back to the metal, it clearly "disappears", but if in
solution, the vendor is supposed to be clever enough to make it not re-
deposit. The old style rosin fluxes "dissolved" the oxide, by reacting a
(rosin) fatty acid, with the metal in the oxide, and it got pushed aside by
the incoming solder.
Which mode your flux works in, clearly depends on which flux you use.
Many fluxes use both modes.
Rudy Sedlak
RD Chemical Company
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|