Run down to your local hardware or craft store and pick up a hot
melt glue gun and glue sticks. Use the milky white opaque sticks, they
are more pliable when hardened and should be fairly easy to remove if
required. The amber sticks are mush stiffer and have poor/less adhesion
on smooth surfaces, mainly used for cardboard and wood (porous)
surfaces. Hurry, hurry, before the stores close (hehehe)....
Mike McMonagle
PCA Process Supervisor
K*Tec Electronics
> -----Original Message-----
> From: Nick Nicolaides [SMTP:[log in to unmask]]
> Sent: Thursday, August 13, 1998 4:36 PM
> To: [log in to unmask]
> Subject: [TN] Adhesive coating for hot wires
>
> Hi Tech Netters
> Our customer does not have time to write new procedures, so we are
> sending
> PWBs' with the attached battery hooked up to the PWB. The battery is
> not hot
> until the PWB is plugged into a mother board. Thus only a small amount
> of
> leakage is occurring during transit. The wires go through to the
> solder side
> and cutting them back only protrudes slightly above the board. The
> customer
> wants these wires protected. The customer will not accept tape. We are
> thinking of some type of adhesive. It must dry fast, be reworkable,
> and
> readily available. We need to ship like now. what can we do!
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
> 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
> section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or
> 847-509-9700 ext.312
> ################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|