Hello all,
I've been lurking on the list for awhile, but I thought I'd come
out of hiding to ask some questions.
I want to try some Kleenox "P" to reduce the amount of dross
from our Wave Solder pot. Does anyone out there have any good or bad
experiences with its use? Will its repeated use leave a residue or
contamination in the solder? Are there any downsides that I'm not
thinking of? Lastly, was it cost-effective for you to use?
Thanks in Advance,
Tom Moss
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|