Uralane 5750 (Ciba) and Parylene C (Du Pont) meet most of these
requirements as conformal coatings.
----------
From: Jan Satterfield [SMTP:[log in to unmask]]
Sent: Wednesday, August 12, 1998 2:10 PM
To: [log in to unmask]
Subject: Re: [TN] The ideal eletronic encapsulation material?
I think everyone would like to know the answer to this one! If
anyone
does, please share the response on TechNet!
>-----Original Message-----
>From: Edward Boucher [SMTP:[log in to unmask]]
>Sent: Wednesday, August 12, 1998 2:49 PM
>To: [log in to unmask]
>Subject: [TN] The ideal eletronic encapsulation material?
>
>Greetings Technet,
>
> Dose anyone know of a encapsulating material for electronics, which
can
>meet the majority of these parameters? We have been searching for
about a
>year and have had little success.
>
>The Ideal Encapsulation Material
>
>a. low toxicity
>b. low moisture permeability
>c. no or very low ionic content
>d. low viscosity
>e. low linear shrinkage
>f. low glass transition temperature (Tg)
>g. low Coefficient Of Expansion (CTE)
>h. low embedment stress
>i. high tensile strength
>j. high thermal conductivity
>k. void free
>l. electrical insulation properties
>m. thermal cycling stability
>n. high thermal shock resistance
>o. wide temperature range -55 to 95 degrees C
>p. good chemical and solvent resistance
>q. good adhesion
>r. low cost
>s. ease of processing (application and clean up)
>t. no formation of water
>u. non-corrosive
>v. easily repairable
>
>
>Your help is appreciated...
>
>Ed Boucher
>Engineering R&D Tech.
>K and M Electronics
>413-263-6253
>
>################################################################
>TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
1.8c
>################################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with
following
>text in the body:
>To subscribe: SUBSCRIBE TechNet <your full name>
>To unsubscribe: SIGNOFF TechNet
>################################################################
>Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
section
>for additional information.
>For technical support contact Hugo Scaramuzza at [log in to unmask] or
>847-509-9700 ext.312
>################################################################
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|