Vernon ; good question
if TH ; we saw nothing on 3 year stat charts from field ( may be damaged
, but still works );
VERY different on SMD's , we still validate , vibrate , with occasional
shocking revelations on what the test finds and what it misses .
One classic, Earl mentioned on lucky accident on BGA's knock off on
exactly your subject .
This is the reason why I sift through web in odd times .
Whatever you do , do not buy XRay to find this fractures . You won't .
Even live cycling will not discover the extend of stress .
Now I have to make another revision in procedures with a carrot & stick
behind because it is not quite a human nature to run to Steve reporting
his $ 7000 xx layer achievement has been unduly tested just after ICT
pass .
How do I extend the gospel enforcement from floor (relatively easy) to
store (relatively impossible) I hope somebody will tell me .
Beats me
See you
Paul Klasek
http://www.resmed.com
> ----------
> From: Vernon Presnell[SMTP:[log in to unmask]]
> Sent: Friday, 31 July 1998 2:30
> To: [log in to unmask]
> Subject: [TN] Dropped boards
>
> Does any one have any experience with evaluating the reliability of
> dropped PWB assemblies?
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
> 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
> section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or
> 847-509-9700 ext.312
> ################################################################
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|