Walt,
Try These,
Connor Formed Metal Products 1-800-FOR-EMC1
Insul-Fab 1-800-442-1338
Instrument Specialties 714-579-7100
http://www.instrumentspecialties.com/
BMI 847-934-4700
http://www.bmimetronics.com/
Rubbercraft 1-800-RUBBER-9
http://www.rubbercraftcorp.com
Northwest Etch Technology has been good at making etched prototypes, Tel.
1-800-343-2401
http://www.nwetch.com/
Also here is a page for EMI/RF Buyers guide
http://www.nelsonpub.com/ee/buyguides/emibuyg.htm
J. Mark Elliott
Reliability Engineer, Maxtek Components Corp.
503.627.3641
[log in to unmask]
"TOM HYBISKE" <[log in to unmask]> Wrote:
|
| Good Afternoon List Members,
|
| I'm trying to find a source for those small metal
| containers that
| solder in place over circuitry to prevent emission or
| reception of
| EMI/RFI. Can anyone point me to a US vendor?
|
| Thanks,
| Thomas Hybiske
| General Atronics Corporation
|
"Walt Johnson" <[log in to unmask]> Wrote:
|
| I am interested in information about using pick and place
| to attach shields
| to PCBs in medium to high volume products. We plan to use
| a one piece
| shield with a perforated top. The shield will be about
| 1.5" X 1.5". We
| hope that the perforations will allow us to reflow the
| components under the
| shield.
|
| Any experience with something like this would be very
| helpful.
|
|
| Walt Johnson
| Almaden Valley Technical Management
| 408-268-6744
| Fax 408-268-8071
| [log in to unmask]
|
| ##########################################################
| ######
| TechNet E-Mail Forum provided as a free service by IPC
| using LISTSERV 1.8c
| ##########################################################
| ######
| To subscribe/unsubscribe, send a message to
| [log in to unmask] with following text in the body:
| To subscribe: SUBSCRIBE TechNet <your full name>
| To unsubscribe: SIGNOFF TechNet
| ##########################################################
| ######
| Please visit IPC's web site (http://www.ipc.org) "On-Line
| Services" section for additional information.
| For technical support contact Hugo Scaramuzza at
| [log in to unmask] or 847-509-9700 ext.312
| ##########################################################
| ######
|
|
J. Mark Elliott
Reliability Engineer, Maxtek Components Corp.
503.627.3641
[log in to unmask]
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|