TECHNET Archives

August 1998

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
Subject:
From:
Werner Engelmaier <[log in to unmask]>
Date:
Sun, 30 Aug 1998 10:32:53 EDT
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset=US-ASCII
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Parts/Attachments:
text/plain (49 lines)
Hi Mark,
What you are proposing to do is not a good idea.
First, there is no such thing as a standard 'solder joint
force/shear/peel/pull test.' Because of the large variety of solder joint
geometric variations, there can not be one from this consideration alone.
Second, the solder joint strength, as determined by a lead shearing test, has
no bearing on the reliability of the solder joint, provided the test does not
reveal inadequate wetting.
Third, the fracture surface of the forced solder joints give typically more
information than do the shear-load histories, because the ONLY really
important finding is whether or not adequate wetting has taken place.
Fourth, the reliability in actual use does to a large extent depend on the
heel fillet and the 'bottom flat' wetting; if the foot length is <3W, than
also on the presence of a toe fillet, because short feet 'rock' during thermal
cycling. Side fillets are less important, unless you have wetting problems.
Fifth, make sure that your definition of a 'poor' solder joint corresponds
with ANSI-J-STD-001.

Werner Engelmaier
Engelmaier Associates, L.C.
Electronic Packaging, Interconnection and Reliability Consulting
7 Jasmine Run
Ormond Beach, FL  32174  USA
Phone: 904-437-8747, Fax: 904-437-8737
E-mail: [log in to unmask]

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2