Rick,
Mil-STD-2000A has a bunch of lead tinning requirements. They require a
segregation of the tinning area away from other areas if the flux used is
anything but type R or RMA. They also specify maximum contamination limits
on tinning pots and separate limits on Assembly soldering. If you use a
non-rosin flux you must also provide certain data on cleanliness testing. I
believe it also requires Mil-Std-2000 certification of personnel which may
not be possible for you to get any longer. You may need a waiver for this
one.
If you build to this standard you will want to understand it thoroughly.
Let me know and I'll send you a copy of the standard. My copy of
Mil-Std-2000A is dated 14
February 1991.
Good Luck
Russ Winslow
[log in to unmask]
-----Original Message-----
From: Rick Thompson <[log in to unmask]>
To: [log in to unmask] <[log in to unmask]>
Date: Thursday, August 27, 1998 1:51 PM
Subject: [TN] MIL-2000 Lead Tinning?
>Hi,
>
>We have a customer who is requesting a quote to build PCBAs with a
>requirement for lead tinning & 'single-point' soldering per Mil-2000. He
>knows that Mil-2000 has been superceded but their customer is still
>requiring it. I don't have a copy of Mil-2000 and was wondering if someone
>could briefly tell me what the lead tinning requirements of the spec were,
>was it a requirement at all times or only when solderability testing
failed,
>etc. Also, what the term 'single-point' soldering refers to; I'm not
>familiar with the term.
>
>Thanks.
>
> Rick Thompson
> Ventura Electronics Assembly
> 2665A Park Center Dr.
> Simi Valley, CA 93065
>
> [log in to unmask]
>
> (805) 584-9858 voice
> (805) 584-1529 fax
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|