You can use specific gravity as a measure of the stripper's loading, and
hence change schedule. We use NPS3000 from RBP-Chemelex, a nitric acid
based stripper in an MP-80 tab line. Charts and data on the
specific gravity (loading) vs strip times are available.
Call 1-800-558-0747 and speak to Lois Halloway.
Lenny Kurup
EMX Enterprises Ltd.
################################################################