Dear sir,
Please try the Qualitek solder paste #670S1 for SMT, it is the low flux
residue solder paste. I have experience with it, it pass contaminant test
perform IPC standard by our cutomer. For PTH is Alpha metal, Telecore
plus1.2% flux core, 0.5% dia, this one has passed the test also. For
noclean flux removing please try Alpha metal # EC-7M.
Best regards,
Noppadol S.
At 15:00 24/7/98 -0700, you wrote:
>Hello.
>
> I am needing a way to determine if flux residue from "no - clean" flux
>is a problem with reliablity on fr4 pcbas. IPC standards are unclear and
>suggest test methods that are excessively costly for me. Is there any
>products that may help me determine the contamination level (cheap) or
>do you have "safe" cleaners ?.
>
>Thanks
>
>Cheyenne Noda
>[log in to unmask]
>
>################################################################
>TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
>################################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in the body:
>To subscribe: SUBSCRIBE TechNet <your full name>
>To unsubscribe: SIGNOFF TechNet
>################################################################
>Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
section for additional information.
>For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
>################################################################
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|