Has anyone encountered capacitors cracking due to bulbuous joint formation on wavesolder. We operate a Hollis wavesolder machine with air knife and joints on trailing end of a component are larger than the joints on the leading end. Can this lead to stressing of the capacitors and if so whats the best type of corrective action??