> From: Michael D. Doty <[log in to unmask]>
> To: [log in to unmask]
> Subject: [TN] Dump Criteria for Solder Strip
> Date: Wednesday, July 01, 1998 10:21 PM
>
>
> I'm looking for dump criteria on solder strip in a Tab line. I
> currently dump on board count but would like to know if 1.) There is
a
> copper concentration I could dump to or 2.) it is overkill?
> I can't seem to get any info on this from vendors or other users.
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
> ################################################################
Michael,
Look in Manko's book, I believe he gives a figure.
Frank Komitsky, Jr.
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|