Has anyone had experience with conformal coating over a "no-clean"
flux residue? Right now we are using a Humiseal - 1B73 Acrylic,
and using a water soluble flux. We are in the process of going
outside with this assembly and most of the contract houses that we
have talked with use no clean. thanks
Mark