I wonder how many of you using acid stoper during developing of dry film?
say citric acid. and I would like to hear your comments. For those chemists
out there, I like to know whether it is really possible to titrate a weak
acid with three Ka ?
Oh, by the way, anyone using resist lamintor with two sets of rollers, hot
to hot; Like to try or modify a one, if you have some information, would you
please share with me?