We did some measurements a few years ago on boards coated with four
different solder mask materials, for a project where we were modelling
the reflow soldering process. All came out pretty close to an emmissivity
of 1 for the FR4 laminate, but where there were tracks beneath the solder
mask the emmissivity was around 0.6
David Whalley
At 05:33 PM 7/6/98 -0600, Mark Harrand wrote:
>Technetters,
>
>I'm working on a project that involves radiant heating of a circuit board.
>I need to know the emmitance value for a standard FR-4 board with solder
>mask.
>
>None of my handbooks gives this value, and several internet searches turned
>up nothing. Can anyone help?
>
>
>
>Mark Harrand
>SRC Computers, Inc.
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|