TECHNET Archives

July 1998

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Subject:
From:
Neil Atkinson <[log in to unmask]>
Date:
Wed, 15 Jul 1998 09:41:15 +0100
Content-Type:
multipart/mixed; boundary="---- =_NextPart_000_01BDB0DF.C724B870"
MIME-Version:
1.0
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Neil Atkinson <[log in to unmask]>
Parts/Attachments:
text/plain (646 bytes) , application/ms-tnef (1641 bytes)
Thanks to Ron Hayashi for his reply regarding shelf life of immersion
gold PCBs.

The boards I have experienced problems with are coming up to 18 months
old (I tend to agree with Ron that 6 months is about the maximum shelf
life) but I have also looked at the thickness and quality of plating.
The gold on the board is 0,014 microns thick using XRF equipment (is
this OK?) I thought that seemed quite thin!?

I have witnessed 'pitting' in the nickel layer which, in some cases,
goes right down to the copper.

Can anyone tell me how much nickel / gold should be on the board and
what effect the above would have on solderability / shelf life

Thanks,